Why is the Hole in Aluminum Alloy die Casting should be Less Than 0.25mm?
Posted: 01/18/2017 05:13:23  Hits: 12
We add a lot silicon into aluminum alloy for die casting. When aluminum alloy was condensed in the mold, silicon would float to the surface and form a thin layer of silicon film, which has high hardness and wear resistance. Some designers of OME (Original Equipment Manufacturer) use this feature to transform the hole surface into bearing surface. The thickness of silicon film is usually from 0.2 to 0.9mm. Too much processing would shorten the service life of bearing surface.


Name*
E-mail*
Rate*
Comments*
About the author
Teresa
Teresa
With in-depth knowledge of metallurgy, material science, and manufacturing techniques, Teresa focuses on producing and optimizing high-quality metal components for industries such as automotive, aerospace, and transportation. Her work involves researching and documenting advancements in die-casting technology, and she contributes to academic journals, industry publications, technical manuals, and training materials to educate and inform professionals in the field.

Link To Us|Privacy Policy|Sitemap|Top back to top